Greg Barratt wrote:
 i'm looking to retain a flat finish,

I've used Sodium Silicate (found at a chemical supply store)
Brush it on, wash it off and bake for 30 minutes at 275 degrees.
It seals the pores in the metal. My loop engine block and trans case
still look fresh and clean two years later....yup, my block fit in the
oven!!!