Synonym: "Wasserglas" water glass, it forms a glass-like coating over/in
the cast aluminum. Don't spill it and don't let it dry on anything you
don't want it on. If you ever want it off, you'll need to take it to an
anodizer, for example, that uses an acid fluoride bath for deoxidizing.
Don't ever use a fluoride product yourself if you like your bones. (I am
not talking about fluoridation or special toothpastes, they work, let's
not go there).